doi: 10.2172/4279681
Binary alloys of uranium with 38 elements in the range 0.01 to 1.0 at.% were made. Three alloys havirg nominal compositions of 0.01, 0.1, and 1.0 at.% were made with most of the elements, and in addition, 12 ternary and quaternary alloys were made. The alloys were cast, rolled to 7/8-inch-diameter bars, heat treated, and examined for grain size. (auth)
Metallurgy And Ceramics, Refining, Rolling, Heat Treatments, Elements, Rods, Uranium, Uranium Alloys, Thickness, Grain Size, Casting
Metallurgy And Ceramics, Refining, Rolling, Heat Treatments, Elements, Rods, Uranium, Uranium Alloys, Thickness, Grain Size, Casting
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |