Abstract Selection of steels for petroleum refinery vessels and piping is determined by the most economical combination of code allowable stresses and ability to resist service deterioration under operating conditions. Temperature is a major factor in selection because it effects both strength and corrosion rate; refinery operating temperatures may range from -50 degrees F or lower to 1200 degrees F or higher depending on the process. Hydrogen deteriorates some steels over much of this range but the mechanism of attack varies with temperature. Design stresses for many steels are constant in the range -20 degrees F to 650 degrees F, but at and below atmospheric temperatures ferritic steels may undergo a notch-brittle transition; the probability of this hazard must be recognized. From 650 degrees F to 1200 degrees F, ferritic steels containing up to 9 percent chromium and 1 percent molybdenum resist most forms of deterioration successfully. The higher chromium ferritic steels have little merit. Above 1200 degrees F, and for severely corrosive conditions at lower temperatures, austenitic stainless steels must be used.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |