Transparent alumina with a fine grain size (0.27 μm) was obtained by controlling the heating rate during spark plasma sintering processing. The alumina sintered at 1150 °C with a heating rate of 8 °C/min has a residual porosity of 0.03% and an in-line transmission of 47% for a wavelength of 640 nm. We show that a low heating rate has an effect on the densification and transparency of alumina for sintering at 1150 °C.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 233 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Top 1% | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 1% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Top 1% |