Inorganic UV absorbers which are widely used today were originally designed neither as a UV blocker in coatings applications, nor for wood protection. In recent years however, there has been extensive interest in these compounds, especially with regard to their properties as a UV blocker in coating applications. In this work, we carried out a comparative study to look into some inorganic and organic UV absorbers used in wood coating applications. The aim of this study is to determine the photostabilisation performances of each type of UV absorbers, to seek possible synergies and the influences of different wood species. We have also searched to find eventual correlation between these performances and the influence of UV absorbers on the film properties. Our study has compared the performances of the following UV absorbers: hombitec RM 300, hombitec RM 400 from the Sachtleben Company; transparent yellow and red iron oxides from Sayerlack as inorganic UV absorbers; organic UV absorbers Tinuvin 1130 and Tinuvin 5151 from Ciba Company. The study was carried out on three wood species: Abies grandis, tauari and European oak. The environmental constraints (in particular the limitation of the emission of volatile organic compounds VOCs) directed our choice towards aqueous formulations marketed by the Sayerlack Arch Coatings Company. The results obtained after 800 h of dry ageing showed that the Tinuvins and the hombitecs present better wood photostabilisations. On the other hand in wet ageing, with the hombitec, there are appearances of some cracks and an increase in the roughness of the surface. This phenomenon is absent when the Tinuvins are used. With regard to these results, the thermomechanical analyses relating to the follow-up of the change of the glass transition temperature (Tg) of the various coating systems, show a different behaviour between the two types of absorbers. However, contrary to organic UV absorbers, inorganic ones tend to increase Tg during ageing, and, consequently decrease the flexibility of films. These phenomena can lead to the appearance of cracks found in the case of the wet weathering.
[SPI.GPROC] Engineering Sciences [physics]/Chemical and Process Engineering, [SDV]Life Sciences [q-bio], ABSORBEUR UV, [SDV.IDA] Life Sciences [q-bio]/Food engineering, 620, AGING, [SDV] Life Sciences [q-bio], TRANSPARENT COATING, BOIS DE FEUILLUS, WOOD SURFACE, [SDV.IDA]Life Sciences [q-bio]/Food engineering, UV ABSORBERS, [SPI.GPROC]Engineering Sciences [physics]/Chemical and Process Engineering
[SPI.GPROC] Engineering Sciences [physics]/Chemical and Process Engineering, [SDV]Life Sciences [q-bio], ABSORBEUR UV, [SDV.IDA] Life Sciences [q-bio]/Food engineering, 620, AGING, [SDV] Life Sciences [q-bio], TRANSPARENT COATING, BOIS DE FEUILLUS, WOOD SURFACE, [SDV.IDA]Life Sciences [q-bio]/Food engineering, UV ABSORBERS, [SPI.GPROC]Engineering Sciences [physics]/Chemical and Process Engineering
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 131 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Top 1% | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Top 10% |