doi: 10.1007/bf01289871
Products made from magnesite and chromite with low-impurity oxide concentrations possess better thermal factors than ordinary periclase-spinel refractories: refractoriness under load: 1700°C and above; bending strength at 1300°C 2.5–3 times greater; deformation 3–4 times; and the rate of deformation at steady-state creep is about a half.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 1 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |