doi: 10.1007/bf00866159
1. Straightening of nitrided shafts at 500–520°C for 10–14 h decreases the fatigue limit (24–34%, according to the data obtained with our models). 2. Tempering of nitrided shafts under the same conditions used for straightening decreases the fatigue limit 8%. 3. One method of avoiding residual sag in large nitrided shafts is to nitride continuously rotating shafts. This method has been developed and applied at the Russian Diesel Plant.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |