Nickel powder obtained by reduction from Cuban production waste (PNVK) exhibits good compressibility. Difficult-to-reduce oxide impurities decrease its low-temperature sintering “activity” compared with carbonyl powder and powder reduced from pure nickel oxides. As a result, for sintering PNVK powder higher temperatures (1100–1200°C) are required.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |