AbstractPoly(ester‐imide)s with a regular sequence of aliphatic spacers and aromatic imide mesogens were prepared in two ways. Either aliphatic α,ω‐diacids were condensed with an acetylated diphenol derived from 4‐hydroxyphthalic acid and 4‐aminophenol, or aliphatic α,ω‐diacid dichlorides were condensed with the silylated diphenol. The resulting poly(ester‐imide)s were characterized by elemental analyses, viscosity measurements, microscopy under polarized light, DSC‐ and WAXS measurements. All poly(ester‐imide)s are crystalline materials with a layered supermolecular structure in the solid state. Above the melting point a nematic mesophase exists over a broad temperature range. A pronounced odd‐even effect was found for the temperature of isotropization, but not for the melting points.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 61 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Top 10% |