Fire is one of the most frequent disasters in the world. As bamboo is combustible material, its fire performance greatly limited its structural application. However, study shows that fire safety of bamboo structures can be ensured through reasonable fire design. In this paper, the charring properties of two types of engineered bamboo: laminated bamboo and bamboo scrimber were carefully investigated through numerical study with commercial software ABAQUS. Charring rate was calculated from the simulated 300oC isotherm. The influence of cross-section dimension, fire duration on the charring rate was studied. Two types of engineered bamboo showed similar development rule of charring rate. The charring rate of engineered bamboo decreased slightly with the increase of fire duration.
charring, numerical simulation, engineered bamboo, fire
charring, numerical simulation, engineered bamboo, fire
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |
| views | 9 | |
| downloads | 11 |

Views provided by UsageCounts
Downloads provided by UsageCounts