Metal matrix composite (MMC) bling (bladed ring) for gas-turbine's compressor was developed. The bling was consist of monolithic titanium clad and hoop reinforced MMC core. The MMC core material was using titanium matrix coated fiber. The MMC core's fabrication process included winding of matrix coated fiber (wire) to pre-form and hot press consolidation of stacked pre-forms. The clad and the core were integrated into one piece ring with HIP. The results shows this process can minimize the misalignment and fiber breakage during consolidation. Uniform wire diameter, precise winding, and hot pressing are effective for successful processing. The burst spin strength of bling achieved 89% of coupon tensile strength.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |