Fe doped ZnOthin films with different Fe concentrations have been deposited by Sol-gel method. X-ray diffraction (XRD) confirmed that hexagonal wurtzite structure in all samples. However, the preferential orientation changed from (002) to (101) plane with increase of Fe-doping. Unit cell parameters, ?a? and ?c?, reduced with the enhancing the Fe content up to 5%, which indicated that Fe ions substitute into the lattice of zno. The Raman spectroscopy measurement showed the peaks at 377.33 cm-1, 439.14 cm-1 and 538.76 cm-1 which are the characteristic vibrational modes of zno. The scanning electron microscopic (SEM) images showed irregular shaped grains grown over the substrate surface for pure zno. After Fe doped zno thin films exhibits the spherical and hexagonal structure. UV-Vis spectra of show the decrement the band gap up to 3.18 to 2.92 eVafter the enhancing the Fe concentration.
X- Ray diffraction ZnO UV=Vis Raman Spectroscopy Band gap Crystallite size.
X- Ray diffraction ZnO UV=Vis Raman Spectroscopy Band gap Crystallite size.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |