Abstract Crack propagation tests were carried out on 2024-T3 sheet specimens to study the effects of omitting low-amplitude cycles from the gust-dominated TWIST load sequence (MiniTWIST) and the removal of small load ranges from the manoeuvre-dominated FALSTAFF load sequence (short FALSTAFF). In other tests high-amplitude loads of TWIST and MiniTWIST were truncated at different levels. The results are compared with data from similar test programmes, including crack initiation. Attention is paid to unstationary crack growth retardation and a transient retardation during initial crack growth started by an artificial crack.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 22 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Top 10% | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |