Thermal shock testing of opaque porcelain-body porcelain discs and body porcelain discs was performed on three porcelain products. Significant differences exist between the mean failure temperature differentials, delta T, for the composite opaque-body porcelain discs. The residual tensile stress and the transient tensile stress distribution are more severe for one of the three porcelains tested.
Time Factors, Tensile Strength, Temperature, Thermodynamics, Stress, Mechanical, Dental Porcelain
Time Factors, Tensile Strength, Temperature, Thermodynamics, Stress, Mechanical, Dental Porcelain
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 21 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Top 10% |