Crowns made from an yttria-stabilized tetragonal zirconia polycrystals (3Y-TZP) core with a porcelain veneer have shown high clinical failure rates. Manifestations of clinical failure in veneering ceramic ranges from a single chip to an extended fracture. Core failures are uncommon but usually are catastrophic. This article examines the possible causes of failure in zirconia systems and presents a case report involving the diagnosis and repair of three different types of failure in six 3Y-TZP/porcelain crowns.
Crowns, Dental restoration, Middle Aged, Dental restoration failure, Dental Veneers, Humans, Female, Yttrium, Dental Restoration Failure, Zirconium, Dental porcelain, Human
Crowns, Dental restoration, Middle Aged, Dental restoration failure, Dental Veneers, Humans, Female, Yttrium, Dental Restoration Failure, Zirconium, Dental porcelain, Human
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |