Temperature dependence of heat capacity of native and denatured collagen samples with different content of bound water (6 divided by 27%) has been studied by DSC method in the temperature range from -50 to 150 degrees C. Heat capacity of denatured samples demonstrates a jump of 0.50 J/g.grad. at temperature Tg, which depends on humidity of the sample. It has been shown that Tg value also depends on the heating rate and thermal history. Annealing at the temperature below Tg produces an additional maximum in the temperature dependence on heat capacity. The magnitude of this maximum, as well as the Tg value increase with the annealing time. It is concluded that these properties of heat capacity reflect glass transition in the denatured collagen.
Protein Denaturation, Hot Temperature, Calorimetry, Differential Scanning, Collagen
Protein Denaturation, Hot Temperature, Calorimetry, Differential Scanning, Collagen
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 9 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |