We show a comparative study of the TiO2 ALD with TTIP and either O2 or O2-plasma on Si/SiO2 substrates. In particular we compare the surface morphology and crystalline phase by means of Atomic Force Microscopy (AFM), X-ray Photoelectron Spectroscopy (XPS) and X-ray Absorption Spectroscopy (XAS) for different O2-plasma procedures upon changing the time between cycles and the N2-purging pressure. The AFM images show that already these parameters may induce structural changes in the TiO2 films grown by ALD, with the formation of crystallites with average lateral width varying between 15 and 80 nm. By means of XAS we also found that the crystallites have mixed anatase and rutile crystalline phases and that smaller crystallites have a greater rutile component than the larger ones.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |