This study attempted to polish pure titanium test pieces electrolytically to mirror surface at the size of cast denture frames. Electrolytic polishing of pure titanium could be done on an area of 30 cm2 with a non-aqueous electrolyte. Small pure titanium plates could be polished electrolytically, but a uniformly smooth surface could not be obtained easily with large testpiece. The optimal electrolytic conditions were 30 V for 6 min at 25 degrees C using a solution consisting of 70 ml ethyl alcohol, 30 ml iso-propyl alcohol, 6 g aluminum chloride, and 25 g zinc chloride. The solution was safe and had less restriction of frequency of use.
Titanium, Denture Bases, Ethanol, Surface Properties, 1-Propanol, Electrolysis, Dental Polishing, Zinc, Chlorides, Zinc Compounds, Aluminum Chloride, Aluminum Compounds, Aluminum
Titanium, Denture Bases, Ethanol, Surface Properties, 1-Propanol, Electrolysis, Dental Polishing, Zinc, Chlorides, Zinc Compounds, Aluminum Chloride, Aluminum Compounds, Aluminum
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |