To compare the metal-ceramic bonding strength of different ceramic alloies.30 wax sheets were divided into 6 groups at random. Each group included 5 sheets. After being invested conventionally with Bellaves SH,the samples were casted and fused with porcelain.The metal-ceramic bonding strength was evaluated.The highest bonding strength was found in Bio Herador N alloy, and then in TILITE alloy and Heraenium S alloy respectively. Bio Herador N alloy and TILITE alloy all had significant differences of the bonding strength before and after treatment (P0.05).The bonding strength of precious metal-ceramic was higher than that of non-precious metal-ceramic.Pre-oxygen treatment can improve the metal-ceramic bonding strength of Bio Herador N alloy and TILITE alloy,but it had no effect on the metal-ceramic bonding strength of the Heraenium S alloy.
Dental Stress Analysis, Materials Testing, Dental Bonding, Metal Ceramic Alloys
Dental Stress Analysis, Materials Testing, Dental Bonding, Metal Ceramic Alloys
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |