In this study, the experiments of warm deep drawing were done with heated die, and with heated die, and blankholder, and cooled punch in order to investigate the formability of AZ31 magnesium alloy sheet in warm deep drawing. For this, warm deep drawing experiments were executed under various temperatures and punch velocities. The results of warm deep drawing with heated die showed that fracture occurred around the punch part at punch velocity of 75mm/min and punch stroke of 10mm under temperature range of 373-523K, but did not occur under temperature range of 548-673K even punch stroke of 25mm. And fracture at the punch stroke of 25mm and the temperature of 523K did not occur under the punch velocity of 30mm/min, but occurred under punch velocity of 75 and 125mm/min. Also warm deep drawing with heated die and blankholder, and cooled punch showed that the temperature range happening maximum height under punch velocity of 10-100mm/min was around 498-523K. Finally, with heating and cooling technique necking of AZ31 magnesium alloy occurred at punch shoulder part under the temperature range of 293-423K, but at die wall part under the temperature range of 473-573K.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |