doi: 10.4271/910135
<div class="htmlview paragraph">The dynamic fatigue data for two different cordierite ceramic wall-flow diesel filter compositions, EX-54 and EX-66, are obtained at 200° and 400°C using the 4-point bend test. These compositions offer larger mean pore size and experience lower pressure drop than the EX-47 composition, and hence are more desirable for certain applications. Their fatigue behavior in the operating temperature range is found to be equivalent or superior to that of EX-47 composition which helps promote filter durability. The fatigue data are used to arrive at a safe allowable stress, which would ensure the required 290K vehicle mile durability. The paper also discusses the impact of mean pore size on high temperature strength and fatigue properties and their effect on filter durability.</div>
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 12 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Top 10% |