In order to improve the hardness of commercial bone china, we attempted to control the glost firing temperature and apply a chemical strengthening process. When the glost firing time was longer or its temperature was higher than normal conditions, the hardness was improved by approximately 5%. The chemical strengthening process also enhanced the hardness of the glaze by more than 13% compared with bone china. It is believed that the enhancement of the hardness of the glaze was related to the development of residual compressive stress in the glaze due to 1) the increase in the calcium phosphate phase in the interface layer between the body and the glaze after firing, and 2) the increase of the K+ concentration on the glaze surface during the chemical strengthening process.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 1 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |