doi: 10.4095/302093
Asphalt, pitches, solvent refined coal (SRC) and petroleum coke were added to coke oven charges in an attempt to make good metallurgical coke from Canadian coal of poor coking quality. Asphalt, pitches and SRC were added to a low fluid western Canadian coal of medium volatile bituminous rank, and the blends coked in a technical-scale moveable wall test oven having a 230-kg charge capacity. Pitches improved coke tumble test indices, the principal coke quality parameter related to blast furnace performance. Varying levels of petroleum coke were added to an eastern Canadian coal of high volatile bituminous rank, and the blends, some partially briquetted, were carbonized in a test oven. Tumble indices of coke from the partially briquetted charges approached an acceptable level. These investigations confirm that petroleum products as well as coal derivative can play a useful part in the production of a:netallurgical strength coke from poor or non-coking coals.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |