This paper examines the effects of different crumb rubber sources on Crumb Rubber Modified (CRM) binder failure temperatures as defined by the Strategic Highway Research Program (SHRP) testing procedures. Focus is on identifying crumb rubber properties that affect the rutting susceptibility of the CRM binders. Four crumb rubber sources' properties are identified by: grinding procedure, elemental analysis, and glass transition temperature.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 21 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Top 10% | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |