Refractory sulphide–barite ore was reduced with carbon in order to release lead, zinc, and copper sulphide from barite-pyrite base. Mineralogical investigations showed that due to the complex structural-textural relationships of lead, copper and zinc minerals with gangue minerals, it is not possible to enrich the ore using the conventional methods of mineral processing. The influence of temperature and time was studied to optimize the conditions, and to determine the kinetics of the barite reduction. The maximum removal of barite from ore was 96.7% at 900oC after 180 min. Chemically controlled kinetic model showed the best compliance with the experimental data. An activation energy of 142 kJ/mol was found.
kinetic of barite reduction, refractory sulphide-barite ore
kinetic of barite reduction, refractory sulphide-barite ore
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 1 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |
| views | 46 | |
| downloads | 50 |

Views provided by UsageCounts
Downloads provided by UsageCounts