Physicochemical properties of pozzolan Portland cement were compared to ProRoot MTA and MTA BIO. To test the pH, the samples were immersed in distilled water for different periods of time. After the pH analysis, the sample was retained in the plastic recipient, and the electrical conductivity of the solution was measured. The solubility and radiopacity properties were evaluated according to specification 57 of the American National Standard Institute/American Dental Association (ANSI/ADA). The statistical analyses were performed using ANOVA and Tukey’s test at a 5% level of significance. Pozzolan Portland cement exhibited pH and electrical conductivity mean values similar to those of the MTA-based cements. The solubilities of all tested materials were in accordance with the ANSI/ADA standards. Only the MTA-based cements met the ANSI/ADA recommendations for radiopacity. It might be concluded that the pH and electrical conductivity of pozzolan Portland cement are similar to and comparable to those of MTA-based cements.
Research Article
Research Article
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 2 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |