It has been found that the amorphous powder of a transition metal - metalloid alloy can be prepared by the spark erosion technique. The powder consists of roughly spherical particles whose diameters are ranging from 0.5 μm to 30μm. The preparation procedure of the powder is described and its magnetothermal characteristics and the crystallization behaviours are discussed.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 45 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Top 10% | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 1% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |