Measurements of total power loss and domain-wall spacing have been made on individual grains in polycrystalline specimens of commercial grain-oriented 3% silicon-iron material. The loss-per-cycle against frequency characteristic of a grain is found to consist of discrete linear portions, which correspond to different domain-wall spacings. These changes in domain pattern result in a lower value of static hysteresis loss than expected and, therefore, a larger proportion of the total power loss must be attributed to the anomalous loss. From domain observations, it is concluded that a part of the anomalous loss is due to nonuniform flux distribution in the material and the overloading of the well-oriented grains.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 11 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |