Textured (1 − x − y)Bi0.5Na0.5TiO3–(x)BaTiO3–(y)K0.5Na0.5NbO3 ceramics have been produced by tape casting with pure-phase Bi0.5Na0.5TiO3 templates. Rietveld texture refinement was used to analyze the crystallographic preferred orientation of the fired ceramics. The effect of poling field on d33 was investigated for applied fields between 0–8 MV m−1 for pure Bi0.5Na0.5TiO3 and 0–5 MV m−1 for Bi0.5Na0.5TiO3 alloys, and compared against randomly oriented samples. Texturing enhanced the piezoelectric response of all measured compositions with Bi0.5Na0.5TiO3–(5)BaTiO3 reaching a maximum d33 of 245 pC N−1.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 32 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Top 10% | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Top 10% |