Abstract The solubility of C in solid Cu was determined in the temperature range 1143–1293 K. Layers of C were vapour deposited onto high-purity Cu slices, which were annealed for 72 and 240 h at different temperatures. The C content in the samples was determined by means of combustion analysis. A Henrian behaviour for the carbon activity in the interstitial solid solution was observed.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 285 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Top 1% | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 1% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Top 10% |