SEM and TEM investigations revealed that the chromate coating developed rapidly over the macroscopic alloy surface. The coating thickness increased over the immersion period employed in this study and was about 50 nm and 200 nm for coatings formed after 30 s and 120 s respectively. The coating is composed of chromium compounds with aluminium compounds probably concentrated at the alloy/coating interface.
540, TP Chemical technology, 620
540, TP Chemical technology, 620
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 14 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Top 10% | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |