doi: 10.1007/bf01913853
Results are presented on: (a) the nonisothermal degradation of nitrile-butadiene rubber (NBR) from TG, DTG and DTA data; (b) the accelerated isothermal thermal degradation of NBR at 80°, 90° and 105° from the change in weight versus time data; (c) the accelerated isothermal thermal degradation of NBR at 80°, 90° and 105° from the change in relative elongation at break with time.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 19 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |