The authors have investigated aluminosilicate fiber with organosilicon binder. They show that a rise in pressing pressure from 5 to 50 kPa, a rise in temperature from 300 to 500°C, and a rise in treatment time from 15 to 60 min enables us to obtain products with apparent densities from 0.4 to 0.65 g/cm3.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 0 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |