The porosity and strength of specimens of fused MgO obtained by induction smelting in cold crucibles and having ≤1% impurities is significantly increased by the addition of 1% CeO2, 5% ZrO2, and 20% of the vibromilled component plus 5% Y2O3. An addition of 5% Y2O3 has the greatest effect on the sintering characteristics of the MgO·Al2O3 specimens. A significant improvement in the characteristics of the materials is observed with an increase in the pressing pressure of the specimens from 100 to 200 MPa.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 3 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |