doi: 10.1007/bf00814689
1. Preliminary heating to 1300–1440°C and hardening of medium-and high-carbon steels containing titanium and nitrogen shows a considerable effect on austenite grain growth during subsequent heating. During this heating to 1100°C the grain actually does not grow but at higher temperatures up to 1320°C its retarded growth is observed. A rise in the preliminary heating temperature ensures an increase in the temperature range of retarded austenite grain growth. 2. Annealing at 600–700°C and normalization of steel even after high-temperature heating have no effect on grain growth during repeated heating.
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 2 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Average | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Average | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Average |