doi: 10.1002/pc.21165
AbstractPoly lactic acid (PLA)/Banana fiber (BF) biocomposites were fabricated employing melt blending technique followed by compression molding. BF were surface‐treated by NaOH and various silanes viz. 3‐aminopropyltriethoxysilane (APS) and bis‐(3‐triethoxy silyl propyl) tetrasulfane (Si69) to improve the compatibility of the fibers within the matrix polymer. Mechanical tests revealed an increase of tensile strength to the tune 136% and impact strength to 49% as compared with the untreated biocomposite. Thermal properties of the composites have been evaluated using DSC and TGA. DSC thermograms revealed an increase in the melting transitions thus revealing effective fiber/matrix interface. The thermal stability in the biocomposites also increased in case of banana fiber treated with Si69. Viscoelastic measurements using DMA confirmed an increase of storage modulus and low damping values in the silane treated biocomposites. Biodegradation studies in the biocomposites have been investigated in B. cepacia medium through morphological and weight loss studies. POLYM. COMPOS., 2011. © 2011 Society of Plastics Engineers
| citations The total number of citations received by all articles of the researcher of interest. | 92 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Top 1% | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 10% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Top 10% |