In this work, high density Waspaloy® specimens were produced using specially assembled laboratory equipment by Selective Laser Melting (SLM). SLM of Waspaloy® powder was performed using a high power pulsed Nd:YAG laser. The laser parameters pulse energy (J), pulse width (ms), repetition rate (Hz) and scan speed (mm/min) were varied. Process parameter optimization was achieved using factorial analysis to investigate the relationship between specific processing parameters and the formation of Waspaloy® specimens. The optimized processing parameters produced Waspaloy® specimens that were 99.3 % dense. The resultant laser melted specimen’s height, width and contact angles were measured. Specimens were also observed for the occurrence of porosity.
Selective Laser Melting
Selective Laser Melting
| selected citations These citations are derived from selected sources. This is an alternative to the "Influence" indicator, which also reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | 209 | |
| popularity This indicator reflects the "current" impact/attention (the "hype") of an article in the research community at large, based on the underlying citation network. | Top 1% | |
| influence This indicator reflects the overall/total impact of an article in the research community at large, based on the underlying citation network (diachronically). | Top 1% | |
| impulse This indicator reflects the initial momentum of an article directly after its publication, based on the underlying citation network. | Top 10% |