publication . Article . 2001

Kinetics of manganese in MAG/MIG welding with a 18/8/6 wire

Tušek, Janez;
Open Access English
  • Published: 01 Jun 2001 Journal: Revista de Metalurgia (issn: 0034-8570, eissn: 1988-4222, Copyright policy)
  • Publisher: Consejo Superior de Investigaciones Científicas
Abstract
The paper deals with a study of MAG/MIG welding of low-alloy ferritic steel and highalloy austenitic steel with a 18/8/6 wire. Manganese burn-off from the wire in welding a single-V butt weld was studied. It was found that manganese burns off in the arc during melting of a droplet at the wire end, and from the weld pool during weld formation. The range of manganese burn-off depends mainly on the type of shielding gas used and the arc length, i.e., from the arc voltage. The manganese burn-off increases with an increase of the content of active gases, i.e., CO<sub>2</sub> and O<sub>2</sub>, in the neutral gas, i.e., argon. It also increases...
Subjects
free text keywords: MAG/MIG welding, Manganese, Shielding gas, Burn-off, Black-white welding, </keyword><keyword>Soldadura MAG/MIG, Manganeso, Gas de protección, Consumo, Soldeo blanco-negro;, Mining engineering. Metallurgy, TN1-997
Download from
Powered by OpenAIRE Open Research Graph
Any information missing or wrong?Report an Issue